Repair method of printing rollers

Printing roller surface protection should take newspaper wrap, placed ventilation and shade. Printing rollers usually occurs in a work project wear, holes and other phenomena, if you replace new roll, cost too much, and affect the production schedule. Rubber repair repair repair process can be used. 1, surface treatment: mending touch hair, clean, cleaning, degreasing, and dry. 2, curing curing 4-6 hours can be used for 48 hours to reach maximum strength. 3, adhesive, rubber curing agent for PuTTY white agents in Group b a group of iron to quickly mix (A:B=1:1), and then down to where you want the patch smooth.